Title:
LUMINESCENT GLASS ELEMENT, THE PREPARING METHOD THEREOF AND THE METHOD FOR LUMINESCENCE USING THE ELEMENT
Document Type and Number:
WIPO Patent Application WO/2010/148569
Kind Code:
A1
Abstract:
A luminescent glass element comprising a luminescent glass body is provided. A metal film with metal micro structure is formed on the surface of the luminescent glass body having a composition of aM2O•bY2O3•cSiO2•dPr2O3, wherein M is alkali metal, a, b, c and d stand for molar quantities, a is 25-60, b is 1-30, c is 20-70 and d is 0.001-10. A method of preparing the luminescent glass element and a method for luminescence using the element are also provided. The luminescent glass body in the invention has a metal film, which can raising luminous efficiency of the luminescent glass body. The element can be used in light emitting device with ultra high brightness and high speed.
More Like This:
JP4591862 | Luminescent glass article and its manufacturing method |
JP3157000 | [Title of Invention] Optical Waveguide |
JPH0388741 | GLASS FOR DOSIMETER |
Inventors:
ZHOU MINGJIE (CN)
MA WENBO (CN)
LIU YUGANG (CN)
MA WENBO (CN)
LIU YUGANG (CN)
Application Number:
PCT/CN2009/072467
Publication Date:
December 29, 2010
Filing Date:
June 26, 2009
Export Citation:
Assignee:
OCEANS KING LIGHTING SCIENCE (CN)
ZHOU MINGJIE (CN)
MA WENBO (CN)
LIU YUGANG (CN)
ZHOU MINGJIE (CN)
MA WENBO (CN)
LIU YUGANG (CN)
International Classes:
C03C4/12; H01J63/00; C09K11/79
Foreign References:
CN1805105A | 2006-07-19 | |||
CN101442089A | 2009-05-27 | |||
US3523091A | 1970-08-04 | |||
CN101071751A | 2007-11-14 | |||
US20010048966A1 | 2001-12-06 |
Other References:
See also references of EP 2408000A4
Attorney, Agent or Firm:
SHENZHEN ZHONGYI PATENT AND TRADEMARK OFFICE (Old Special Zone Newspaper BuildingNo. 1014, Shennan Rd., C.,Futia, Shenzhen Guanagdong 8, CN)
Download PDF: