Abstract:
A machine part (10) according to one embodiment of the present invention is formed from a titanium alloy. The titanium alloy contains a primary α phase and a secondary α phase. The area ratio of the primary α phase in the titanium alloy is 1% or more but less than 10%. The titanium alloy is a Ti-6Al-4V alloy.
More Like This:
Inventors:
MIZUTA KOHEI (JP)
OHKI CHIKARA (JP)
OHKI CHIKARA (JP)
Application Number:
PCT/JP2018/033176
Publication Date:
March 14, 2019
Filing Date:
September 07, 2018
Export Citation:
Assignee:
NTN TOYO BEARING CO LTD (JP)
International Classes:
C22C14/00; C22F1/18; C22F1/00
Domestic Patent References:
WO2016013566A1 | 2016-01-28 |
Foreign References:
JPS61179832A | 1986-08-12 | |||
JPS62127442A | 1987-06-09 | |||
JP2010255023A | 2010-11-11 | |||
JPS62284060A | 1987-12-09 | |||
JPS484321A | ||||
JPH1150227A | 1999-02-23 | |||
US4975125A | 1990-12-04 | |||
US4898624A | 1990-02-06 |
Other References:
NOZUE, AKIRA ET AL.: "Hydrogen Embrittlement Behavior of Structure Controlled Ti- 6A1-4V Alloy", JOURNAL OF THE JAPAN INSTITUTE OF METALS AND MATERIALS, vol. 51, no. 8, 1987, pages 730 - 736, XP055581872, ISSN: 0021-4876
Attorney, Agent or Firm:
FUKAMI PATENT OFFICE, P.C. (JP)
Download PDF:
Previous Patent: MAGNESIUM-CONTAINING COLORLESS TRANSPARENT BEVERAGE
Next Patent: RECONFIGURATION CIRCUIT
Next Patent: RECONFIGURATION CIRCUIT