METHOD FOR EXTRACTION, ENRICHMENT AND RECOVERY OF RARE EARTHS FROM LOW-CONCENTRATION RARE EARTH SOLUTION
Document Type and Number:
WIPO Patent Application WO/2018/028543
Kind Code:
A1
Abstract:
A method for extraction, enrichment and recovery of rare earths from a low-concentration rare earth solution, using a non-saponification organic extractant to perform centrifugal extraction, obtaining an organic phase containing rare earths and a raffinate; using an inorganic acid to perform centrifugal back-extraction on the organic phase containing rare earths, obtaining a rare earth enriched liquid. Low-concentration rare earth solution indicates a rare earth solution having REO concentration of 0.05-8g/L. Single or dual coupled centrifugal extraction is performed, at an extraction mixing time of 5-60s. The present method has simple operation, protects the environment, and has a high rare earth recovery rate.

Inventors:
HUANG XIAOWEI (CN)
FENG ZONGYU (CN)
ZHAO LONGSHENG (CN)
DONG JINSHI (CN)
WANG LIANGSHI (CN)
XU YANG (CN)
CUI DALI (CN)
Application Number:
PCT/CN2017/096222
Publication Date:
February 15, 2018
Filing Date:
August 07, 2017
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
GRIREM ADVANCED MAT CO LTD (CN)
International Classes:
C22B59/00; C22B3/26
Foreign References:
CN104294063A2015-01-21
CN101824535A2010-09-08
CN101050488A2007-10-10
EP2910654A12015-08-26
Attorney, Agent or Firm:
KANGXIN PARTNERS, P.C. (CN)
Download PDF: