Abstract:
The present invention comprises: a step of mixing a porous coal and a solvent oil; a step of dewatering a slurry obtained in the mixing step; a step of performing solid-liquid separation on the slurry; and a step of drying a cake obtained in the solid-liquid separation step. An oil component including solvent oil recovered in the solid-liquid separation step and the drying step is returned to the mixing step, and the oil content of the cake in the solid-liquid separation step is adjusted to 15-40wt%.

Inventors:
FURUYA ATSUSHI
TAKAHASHI YOICHI
KINOSHITA SHIGERU
WATANABE HIROKI
Application Number:
PCT/JP2016/072820
Publication Date:
March 23, 2017
Filing Date:
August 03, 2016
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
KOBE STEEL LTD (JP)
International Classes:
C10L5/00
Foreign References:
JPH07233383A1995-09-05
JP2010090296A2010-04-22
JP2008144113A2008-06-26
JP2008144114A2008-06-26
Attorney, Agent or Firm:
EIKOH PATENT FIRM, P.C. (JP)
Download PDF: