Title:
METHOD FOR PREPARATION OF A SUPERALLOY HAVING A CRYSTALLOGRAPHIC TEXTURE CONTROLLED MICROSTRUCTURE BY ELECTRON BEAM MELTING
Document Type and Number:
WIPO Patent Application WO/2015/108599
Kind Code:
A3
Abstract:
The present disclosure provides a method of preparing superalloy metals having a crystallographic texture controlled micro structure by electron beam melting.
More Like This:
JPS58130202 | PRODUCTION OF SINTERED BODY |
JP2517928 | [Title of Invention] Hot Press Device |
JPH05222407 | METHOD AND DEVICE FOR HIGH-FREQUENCY PLASMA SINTERING |
Inventors:
DAS GOPAL (US)
CERNATESCU LULIANA (US)
SHAH DILIP M (US)
CERNATESCU LULIANA (US)
SHAH DILIP M (US)
Application Number:
PCT/US2014/062581
Publication Date:
September 03, 2015
Filing Date:
October 28, 2014
Export Citation:
Assignee:
UNITED TECHNOLOGIES CORP (US)
International Classes:
B22F3/14; B22F7/02
Foreign References:
JPH0292888A | 1990-04-03 | |||
US5314000A | 1994-05-24 | |||
US20110135952A1 | 2011-06-09 | |||
US20130206352A1 | 2013-08-15 | |||
US20090162205A1 | 2009-06-25 |
Other References:
See also references of EP 3065901A4
Attorney, Agent or Firm:
JONES, Joshua, L. et al. (P.O. Box 55874Boston, MA, US)
Download PDF:
Previous Patent: SUBSTRATES AND ASSOCIATED METHODS FOR ELUTION OF NUCLEIC ACIDS
Next Patent: HEADWEAR SUPPORT DEVICE
Next Patent: HEADWEAR SUPPORT DEVICE