Title:
METHOD FOR REFORMING COAL USING PALM RESIDUE
Document Type and Number:
WIPO Patent Application WO/2014/051180
Kind Code:
A1
Abstract:
The method of the present invention involves directly coating coal with a heavy distillate without using solvent oil, thus saving energy and reforming low-rank coal into high-rank coal having a high calorific value and minimizing water reabsorption and spontaneous combustion in an economically advantageous manner. The present invention provides a method for reforming coal, comprising: a step of grinding coal; a step of uniformly mixing the ground coal and palm residue; a dry-stabilization step of dissolving the palm residue mixed with the coal so as to coat the surface of the coal and simultaneously drying to remove the moisture from the coal; a step of cooling the coal coated with the palm residue in the dry-stabilization step; and a step of molding the cooled coal.

Inventors:
LEE SI-HYUN (KR)
NHO NAM-SUN (KR)
MOON SEUNG-HYUN (KR)
KIM SANG-DO (KR)
CHUN DONG-HYUK (KR)
RHIM YOUNG-JUN (KR)
LIM JEONG-HWAN (KR)
CHOI HO-KYUNG (KR)
YOO JI-HO (KR)
CHOI YOUNG-CHAN (KR)
LEE DONG-WOOK (KR)
RYU IN-SOO (KR)
LEE SEUNG-JAE (KR)
WOO JE KYOUNG (KR)
Application Number:
PCT/KR2012/007904
Publication Date:
April 03, 2014
Filing Date:
September 28, 2012
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
KOREA ENERGY RESEARCH INST (KR)
International Classes:
C10L9/10; C10L5/04
Foreign References:
JPH093457A1997-01-07
JPH07233380A1995-09-05
KR100960793B12010-06-03
Attorney, Agent or Firm:
MOON, Hwan-Goo (Nonhyeon-ro 412Gangnam-gu, Seoul 135-921, KR)
Download PDF: