The present invention provides a polyester resin having, in the main chain, a 2,5-furandicarboxylic acid unit and a cyclohexanedimethanol unit, having a high molecular weight, having heat resistance and hydrolysis resistance, and having excellent mechanical properties and melt thermal stability. In addition, this invention provides a production method for a polyester resin having a high reaction rate and the above-described properties. Provided is a polyester resin having, as main constituents, a 2,5-furandicarboxylic acid unit and a 1,4-cyclohexanedimethanol unit and satisfying the following conditions (I) and (II). (I) The reduced viscosity (ηsp/c) is at least 0.7 dL/g. (II) The total amount of cyclovinylidene ends and methylcyclohexene ends is up to 80 µeq/g.
More Like This:
WO/2005/103111 | POLY(ISOSORBID OXALATE) RESIN |
JP2005518469 | Biodegradable polymer material for bioclinical applications |
JPS61183333 | THERMOPLASTIC RESIN COMPOSITION |
Inventors:
SHIRAHAMA RIE (JP)
HITOMI TATSUYA (JP)
KASAI ATSUSHI (JP)
HITOMI TATSUYA (JP)
KASAI ATSUSHI (JP)
Application Number:
PCT/JP2016/075716
Publication Date:
March 09, 2017
Filing Date:
September 01, 2016
Export Citation:
Assignee:
MITSUBISHI CHEM CORP (JP)
International Classes:
C08G63/672; C08G63/80; C08K3/00; C08K5/098; C08K5/13; C08K5/1515; C08K5/29; C08K5/36; C08K5/49; C08L67/02
Domestic Patent References:
WO2013055860A1 | 2013-04-18 |
Foreign References:
JP2011208008A | 2011-10-20 | |||
JP2016102173A | 2016-06-02 | |||
CN105754077A | 2016-07-13 | |||
JP2008291244A | 2008-12-04 | |||
JP2013053270A | 2013-03-21 | |||
JP2011518235A | 2011-06-23 | |||
JP2011520005A | 2011-07-14 | |||
JP2008007750A | 2008-01-17 |
Other References:
See also references of EP 3345953A4
Attorney, Agent or Firm:
KAWAGUCHI, Yoshiyuki et al. (JP)
Download PDF: