Title:
POWDER METALLURGY TITANIUM ALLOYS
Document Type and Number:
WIPO Patent Application WO/2017/045146
Kind Code:
A1
Abstract:
A sintered Ti alloy comprising: 4 to 6 wt. % iron; 1 to 4 wt. % aluminium or 1 to 3 wt. % copper; >0 to 0.5 wt. % silicon; >0 to 0.3 wt. % boron; >0 to 1 wt. % lanthanum, and the balance being titanium with incidental impurities. In the associated powder metallurgy formation process, the boron and lanthanum content is preferably introduced into a blended powder mixture in the form of lanthanum boride (LaB6).
Inventors:
YANG YAFENG (AU)
QIAN MA (AU)
LUO SHUDONG (AU)
SUN JIFENG (CN)
HUANG AIJUN (CN)
QIAN MA (AU)
LUO SHUDONG (AU)
SUN JIFENG (CN)
HUANG AIJUN (CN)
Application Number:
PCT/CN2015/089698
Publication Date:
March 23, 2017
Filing Date:
September 16, 2015
Export Citation:
Assignee:
BAOSHAN IRON & STEEL (CN)
International Classes:
C22C1/04; C22C14/00
Foreign References:
KR20130142800A | 2013-12-30 | |||
CN101962721A | 2011-02-02 | |||
CN104404300A | 2015-03-11 | |||
JP2002206124A | 2002-07-26 |
Attorney, Agent or Firm:
SHANGHAI PATENT & TRADEMARK LAW OFFICE, LLC (CN)
Download PDF: