Abstract:
A rare earth sintered magnet which comprises 12.0 atomic % to 15.0 atomic % of a rare earth element (which is at least one element selected from the group consisting of Nd, Pr, Gd, Tb, Dy and Ho and contains Nd and/or Pr in an amount of 50 % or more), 5.5 atomic % to 8.5 atomic % of boron (B), a prescribed amount of an additive metal A, and the balanced amount of iron (Fe) and inevitable impurities. The prescribed amount of an additive metal A is at least one of 0.005 atomic % to 0.30 atomic % of silver (Ag), 0.005 atomic % to 0.40 atomic % of nickel (Ni) and 0.005 atomic % to 0.20 atomic % of gold (Au).

Inventors:
MORIMOTO HIDEYUKI (JP)
ODAKA TOMOORI (JP)
Application Number:
PCT/JP2006/314076
Publication Date:
January 25, 2007
Filing Date:
July 14, 2006
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
NEOMAX CO LTD (JP)
MORIMOTO HIDEYUKI (JP)
ODAKA TOMOORI (JP)
International Classes:
H01F1/08; B22F3/02; C22C33/02; C22C38/00; H01F1/053
Foreign References:
JPH04293206A1992-10-16
JPH07272929A1995-10-20
JPS63241141A1988-10-06
JPS63241142A1988-10-06
JPS61221353A1986-10-01
JPH04133406A1992-05-07
JPS59204211A1984-11-19
JPH04343204A1992-11-30
JPH0562814A1993-03-12
JPH09270310A1997-10-14
Attorney, Agent or Firm:
OKUDA, Seiji (10th Floor Osaka Securities Exchange Bldg., 8-16, Kitahama 1-chome, Chuo-k, Osaka-shi Osaka 41, JP)
Download PDF: