Abstract:
A reduction roasting method for iron ore, which provides an approach in which twice reduction roasting is carried out on low-grade difficultly-selected iron ore such as red soil josephinite and iron-aluminum-silicon associated ore by means of a shaft kiln and a rotary kiln, and reduced iron with low cost is directly produced, and the low-grade difficultly-selected iron ore is comprehensively utilized. In the method, coal carbon is directly used as a fuel and a reducing agent, and coke and coal gas are not needed; aluminum oxide is easily and economically extracted; a main component of tailings is calcium silicate, and the tailings can be directly used; no solid waste is produced. By means of the method, low-grade difficultly-selected iron ore is comprehensively utilized, and economic value is high.
More Like This:
JPS5660130 | SPEED CONVERTING CIRCUIT |
JP5862305 | Smoke ash treatment method |
JPH03188228 | METHOD FOR RECOVERING METAL |
Inventors:
LI GUIGEN (CN)
TANG WENLIN (CN)
TANG WENLIN (CN)
Application Number:
PCT/CN2016/092770
Publication Date:
May 11, 2017
Filing Date:
August 01, 2016
Export Citation:
Assignee:
SHENZHEN JINMEIWEI ELECTRON CO LTD (CN)
International Classes:
C22B1/02
Domestic Patent References:
WO2010085635A2 | 2010-07-29 |
Foreign References:
CN105369034A | 2016-03-02 | |||
CN203683618U | 2014-07-02 | |||
CN104195278A | 2014-12-10 | |||
CN203782198U | 2014-08-20 | |||
CN201555450U | 2010-08-18 |
Attorney, Agent or Firm:
YOGO PATENT & TRADEMARK AGENCY LIMITED COMPANY (CN)
Download PDF: