ROLLED STEEL FOR CRACKED CONNECTING RODS
Document Type and Number:
WIPO Patent Application WO/2016/059664
Kind Code:
A1
Abstract:
A rolled steel for cracked connecting rods according to the present embodiment contains, in mass percent, 0.30 to 0.40% of C, 0.60 to 1.00% of Si, 0.50 to 1.00% of Mn, 0.04 to 0.07% of P, 0.04 to 0.13% of S, 0.10 to 0.30% of Cr, 0.05 to 0.14% of V, 0.15% (exclusive) to 0.20% (inclusive) of Ti, and 0.002 to 0.020% of N, and can optionally contain Cu, Ni, Mo, Pb, Te, Ca, and Bi, the balance being Fe and impurities. fn1 defined by the formula (1) is 0.65 to 0.80. The ratio of the V content in large precipitates having a particle size of not less than 200 nm to the V content in the steel is not more than 70%, and the ratio of the Ti content in the large precipitates to the Ti content in the steel is not less than 50%. fn1 = C + Si/10 + Mn/5 + 5Cr/22 + (Cu + Ni)/20 + Mo/2 + 33V/20 - 5S/7 (1)

Inventors:
TAKASUGA MOTOKI (JP)
MIYAKOSHI YUSUKE (JP)
HASEGAWA TATSUYA (JP)
MATSUDA HIDEKI (JP)
KAWAKAMI MASASHI (JP)
SAITO ISAMU (JP)
Application Number:
PCT/JP2014/005274
Publication Date:
April 21, 2016
Filing Date:
October 17, 2014
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
NIPPON STEEL & SUMITOMO METAL CORP (JP)
HONDA MOTOR CO LTD (JP)
International Classes:
C22C38/00; C21D8/06; C22C38/60
Domestic Patent References:
WO2012164710A12012-12-06
Foreign References:
JP2014025105A2014-02-06
JP2010180473A2010-08-19
JP2004277838A2004-10-07
JP2004277817A2004-10-07
KR20100049264A2010-05-12
Attorney, Agent or Firm:
ASCEND IP LAW FIRM (JP)
アセンド patent business corporation (JP)
Download PDF: