Abstract:
A soft-magnetic iron composite powder for use in producing a soft-magnetic composite material having a high resistivity and a low iron loss, the powder comprising a soft-magnetic iron powder and an insulating coating film formed on the surface of the powder by the deposition of a magnesium-containing oxide. When the average particle diameter and the BET value of the soft-magnetic iron powder are expressed by D150 and BET1, respectively, then the soft-magnetic iron powder satisfies the requirements that D150 is 50-300 µm and BET1 D150 is 1.81-2.65. A powder collected by sieving the soft-magnetic iron powder with a sieve having a mesh value which is 1/2 the D150 satisfies the requirement BET2 D250 = 1.50-2.00, wherein D250 and BET2 are the average particle diameter and the BET value of the powder, respectively. Furthermore, the soft-magnetic iron powder has a roundness of 0.840-0.875 and a ruggedness of 0.940-0.948.

Inventors:
UOZUMI GAKUJI (JP)
WATANABE MUNEAKI (JP)
ISHIYAMA KOUICHI (JP)
TANAKA HIROSHI (JP)
IGARASHI KAZUNORI (JP)
MORIMOTO KOICHIRO (JP)
Application Number:
PCT/JP2007/068700
Publication Date:
April 10, 2008
Filing Date:
September 26, 2007
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
MITSUBISHI MATERIALS CORP (JP)
MITSUBISHI MATERIALS PMG CORP (JP)
UOZUMI GAKUJI (JP)
WATANABE MUNEAKI (JP)
ISHIYAMA KOUICHI (JP)
TANAKA HIROSHI (JP)
IGARASHI KAZUNORI (JP)
MORIMOTO KOICHIRO (JP)
International Classes:
B22F1/16; C22C38/00; H01F1/24; H01F1/33
Foreign References:
JP2002317204A2002-10-31
JP2005232535A2005-09-02
JP2001303111A2001-10-31
Attorney, Agent or Firm:
SHIGA, Masatake et al. (Yaesu Chuo-k, Tokyo 53, JP)