Login| Sign Up| Help| Contact|

Patent Searching and Data


Title:
SPARK PLUG INCLUDING ELECTRODES WITH LOW SWELLING RATE AND HIGH CORROSION RESISTANCE
Document Type and Number:
WIPO Patent Application WO/2011/019893
Kind Code:
A3
Abstract:
A spark plug (20) includes a center electrode (24) and a ground electrode (22). The electrodes (22, 24) include a core (26) formed of a copper (Cu) alloy and a clad (28) formed of a nickel (Ni) alloy enrobing the core (26). The Cu alloy includes Cu in an amount of at least 98.5 weight percent, and at least one of Zr and Cr in an amount of at least 0.05 weight percent. The Cu alloy includes a matrix of the Cu and precipitates of the Zr and Cu dispersed in the Cu matrix. The Ni alloy of the clad (28) includes Ni in an amount of at least 90.0 weight percent. The Ni alloy also includes at least one of a Group 3 element, a Group 4 element, a Group 13 element, chromium (Cr), silicon (Si), and manganese (Mn) in a total amount sufficient to affect the strength of the Ni alloy.

Inventors:
MA SHUWEI (US)
LYKOWSKI JAMES D (US)
Application Number:
PCT/US2010/045294
Publication Date:
July 07, 2011
Filing Date:
August 12, 2010
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
FEDERAL MOGUL IGNITION CO (US)
MA SHUWEI (US)
LYKOWSKI JAMES D (US)
International Classes:
H01T13/20; H01T13/32
Foreign References:
US20050023949A12005-02-03
US5497045A1996-03-05
US5395273A1995-03-07
US4949006A1990-08-14
Other References:
See also references of EP 2465173A4
Attorney, Agent or Firm:
STEARNS, Robert, L. et al. (38525 Woodward AvenueSuite 200, Bloomfield Hills MI, US)
Download PDF: