Abstract:
A thermoplastic vulcanizate prepared by a process comprising the steps of dynamically vulcanizing a vulcanizable rubber within a mixture that includes from about 15 to 90 percent by weight of the rubber and from about 10 to about 85 percent by weight of a long-chain branched thermoplastic resin, where the long-chain branched thermoplastic resin is: i) an alpha -olefin polymer; ii) a copolymer of an alpha -olefin and an alpha - omega -olefin diene; or iii) a mixture thereof, where the long-chain branched thermoplastic resin is characterized by a weight average molecular weight from about 100, 000 to about 600,000, a number average molecular weight from about 40,000 to about 200,000, a z-average molecular weight from about 400,000 to about 2,000,000,avis from about 0.2 to about 0.95, and a melt flow rate from about 0.3 to about 30dg/min.
More Like This:
Inventors:
ELLUL MARIA D (US)
SAHNOUNE ABDELHADI (US)
SAHNOUNE ABDELHADI (US)
Application Number:
PCT/US2001/046452
Publication Date:
January 23, 2003
Filing Date:
December 06, 2001
Export Citation:
Assignee:
ADVANCED ELASTOMER SYSTEMS (US)
ELLUL MARIA D (US)
SAHNOUNE ABDELHADI (US)
ELLUL MARIA D (US)
SAHNOUNE ABDELHADI (US)
International Classes:
C08L21/00; C08L23/00; C08L23/16; C08J3/24; (IPC1-7): C08L21/00; C08L23/00; C08J3/24
Domestic Patent References:
WO1998038226A1 | 1998-09-03 |
Foreign References:
US6150467A | 2000-11-21 | |||
US5013793A | 1991-05-07 | |||
EP0849323A1 | 1998-06-24 | |||
EP0393993A2 | 1990-10-24 | |||
US5073597A | 1991-12-17 |
Download PDF: