Abstract:
A composition comprises about 8 to about 10 wt% molybdenum, about 2.8 to about 6 wt% aluminum, up to about 2 wt% vanadium, up to about 4 wt% niobium, with the balance being titanium, wherein the weight percents are based on the total weight of the alloy composition. A method for making an article comprises cold-working a shape from a composition comprising about 8 to about 10 wt% molybdenum, about 2.8 to about 6 wt% aluminum, up to about 2 wt% vanadium, up to about 4 wt% niobium, with the balance being titanium, wherein the weight percents are based on the total weight of the alloy composition; solution heat treating the shape; and cooling the shape.

Inventors:
WU MING H (US)
Application Number:
PCT/US2005/000569
Publication Date:
January 19, 2006
Filing Date:
January 07, 2005
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
MEMRY CORP (US)
WU MING H (US)
International Classes:
C22C14/00; (IPC1-7): C22F1/18; C22C14/00
Domestic Patent References:
WO2004003242A12004-01-08
WO1999045161A11999-09-10
Foreign References:
US6258182B12001-07-10
EP1352979A12003-10-15
US5201967A1993-04-13
EP0263503A11988-04-13
Download PDF: