Abstract:
A method for producing a uranium oxide catalyst body includes the following steps: UO2+x powder, with x≰0.7, having a purity of at least 50% is sintered in a first sintering process to obtain a UO2+y intermediate, where y≰0.25. Then the UO2+y intermediate is oxidized with oxygen and converted in the process into a U3O8−z powder, with z≰1. The U3O8−z powder is pressed to form a blank having a shape that corresponds with the catalyst body to be produced. The blank is sintered in a second sintering process at a temperature of at least 900° C. in an oxygen-containing sintering atmosphere.

Inventors:
Zemek, Martin
Lanceman, Volker
Application Number:
JP2014506914A
Publication Date:
July 10, 2014
Filing Date:
July 25, 2012
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
Areva GmbH
International Classes:
B01J37/14; B01D53/94; B01J23/12
Domestic Patent References:
JP2010533059A2010-10-21
JP2010533058A2010-10-21
JP2010533113A2010-10-21
JP2010533114A2010-10-21
JPS4520974B1
JP2005139440A2005-06-02
JP2000258576A2000-09-22
JP2010533059A2010-10-21
JP2010533058A2010-10-21
JP2010533113A2010-10-21
JP2010533114A2010-10-21
JPS4520974B1
JP2005139440A2005-06-02
JP2000258576A2000-09-22
Foreign References:
WO2010105751A12010-09-23
GB1258413A1971-12-30
US20110180419A12011-07-28
US20110182801A12011-07-28
GB1351803A1974-05-01
WO2010105751A12010-09-23
GB1258413A1971-12-30
US20110180419A12011-07-28
US20110182801A12011-07-28
GB1351803A1974-05-01
Attorney, Agent or Firm:
Iwao Yamaguchi
Hiroshi Yamamoto