To provide a glass fiber-reinforced polypropylene resin pellet having little degradation of mechanical strength under metal contact circumstances and a front part structure of a vehicle obtained from the pellet.
A polypropylene resin (A), a glass fiber (B), a heavy metal deactivator (C), phenolic antioxidant (D), a sulfur antioxidant (E), a hindered amine light stabilizer (F), a phosphorus antioxidant (G) and an ultraviolet absorbent (H) are included. With respect to the weight for each component, (A)/(B), (C)/(A)+(B), (D)/(A)+(B), (E)/(D), (F)/(D), (G)/(D) and (H)/(D) have a specific range respectively. (B) is arranged in parallel with the pellet reciprocally having roughly the same length as a pellet length and the pellet length has a specific range. A limiting viscosity of (A) is made so as to have a specific range.
OBAYASHI YOSHIAKI
INAI ISAMU
ATSUMI MASAKAZU
DENSO CORP
Toru Nakayama
Masayuki Enomoto