Abstract:
[Problem] To provide: a ceramic composite that can have a reduced size or thickness, and can efficiently dissipate heat; and a production method for the ceramic composite. [Solution] This ceramic composite is produced by: a step for preparing a melt comprising at least aluminum oxide and yttrium oxide; a step for bringing either sapphire crystal or ruby crystal into contact with the melt to melt a crystal portion thereof which is in contact with the melt, and to, as a result of the melting, integrate an Al2O3 phase of the crystal and an Al2O3 phase of the aluminum oxide together without a junction interface thereof; and a step for cooling the melt. The produced ceramic composite has at least two oxide phases, i.e., a Y3Al5O12 phase and an Al2O3 phase, as a lamellar structure, wherein an Al2O3 phase, and an Al2O3 phase of either the sapphire crystal or the ruby crystal, are integrated together without a junction interface thereof.
Inventors:
KOTAKI TOSHIRO (JP)
HORIKOSHI FUMIYA (JP)
SUZUKI MASAYUKI (JP)
SHIBATA DAISUKE (JP)
HORIKOSHI FUMIYA (JP)
SUZUKI MASAYUKI (JP)
SHIBATA DAISUKE (JP)
Application Number:
PCT/JP2020/038699
Publication Date:
April 29, 2021
Filing Date:
October 14, 2020
Export Citation:
Assignee:
ADAMANT NAMIKI PREC JEWEL CO LTD (JP)
International Classes:
C30B29/20; C30B11/14; C30B29/22
Foreign References:
JPH11278994A | 1999-10-12 | |||
JP2019056038A | 2019-04-11 | |||
JPS55136197A | 1980-10-23 | |||
US20160326667A1 | 2016-11-10 | |||
CN106676631A | 2017-05-17 |
Download PDF: