Abstract:
The present invention relates to a level wound coil in which a seamless pipe is aligned and wound in multiple layers in a cylindrical shape. The material of the seamless pipe wound around the level wound coil contains between 0.58 and 0.72 mass% of Sn, between 0.005 and 0.035 mass% of Zr, between 0.01 and 0.10 mass% of Fe, and between 0.004 and 0.040 mass% of P, and is a copper alloy made of a balance of Cu and unavoidable impurities. The ratio (t/D) of the thickness (mm) to the outer diameter (mm) of the seamless pipe wound around the level wound coil is 0.040 or less, the tensile strength of the seamless pipe wound around the level wound coil (σB) is at least 280 MPa, the 0.2% proof stress (σ0.2) is 180 MPa or less, and the elongation (δ) is at least 38%. The present invention can provide a seamless pipe that has high strength, can normally perform a hairpin bend, and is formed of copper alloy can be provided.

Inventors:
ANDO TETSUYA (JP)
Application Number:
PCT/JP2013/060825
Publication Date:
October 24, 2013
Filing Date:
April 10, 2013
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
SUMITOMO LIGHT METAL IND (JP)
ANDO TETSUYA (JP)
International Classes:
C22C9/02; B21C47/02; C22F1/08; F28F21/08; C22F1/00
Foreign References:
JP2006274313A2006-10-12
JP2008255381A2008-10-23
JP2005289593A2005-10-20
Other References:
"Improvement of Yield Strength for Heat- Resistance Copper Alloy Tube by Fe Addition", JOURNAL OF THE JRICU, vol. 45, no. 1, 2006, pages 291 - 294