Abstract:
本発明は、35wt%≦Ni≦37wt%、微量≦Mn≦0.6wt%、微量≦C≦0.07wt%、微量≦Si≦0.35wt%、微量≦Cr≦0.5wt%、微量≦Co≦0.5wt%、微量≦Mo<0.5wt%、微量≦S≦0.0035wt%、微量≦O≦0.0025wt%、0.011wt%≦[(3.138×Al+6×Mg+13.418×Ca)−(3.509×O+1.770×S)]≦0.038wt%、0.0003wt%<Ca≦0.0015wt%、0.0005wt%<Mg≦0.0035wt%、0.0020wt%<Al≦0.0085wt%を含み、残部が鉄及び精錬から生じた残留元素である、鉄をベースとした合金に関連する。

Inventors:
Pierre-Louis Rede
Fanny jubanceau
Lolan pannier
Application Number:
JP2016556998A
Publication Date:
May 25, 2017
Filing Date:
March 14, 2014
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
Aperan
International Classes:
C22C38/00; B23K35/30
Domestic Patent References:
JP2008115466A2008-05-22
JPH1161341A1999-03-05
JPH11264055A1999-09-28
JP2008115466A2008-05-22
JPH1161341A1999-03-05
JPH11264055A1999-09-28
Attorney, Agent or Firm:
Atsushi Aoki
Takashi Ishida
Tetsuji Koga
Atsushi Ebiya
Naori Kota
Satoshi Deno
Kenji Kimura