To provide an acrylic resin laminate not spoiling the glass tone touch on the sheet surface even when thermoforming is carried out, and preventing defects generated by adding a large amount of additive, in which the total beam transmittance, haze and light diffused transmittance are so controlled as to be within a certain range, and the transparent touch of crystal glass and the profound touch of frost glass are provided combinedly.
The total beam transmittance of a laminate is 70% or more, and the haze is 80% ore more and the light diffused transmittance is 10% or more, and the laminate is constituted of acrylic resin layers composed of 99-70 wt.% acrylic resin A blended with 1-30 wt.% spherical fine particles B of the 0.02-0.2 absolute value of refractive index difference from the acrylic resin and of 1-100 μm weight average particle diameter laminated on either one of both faces of a base layer.