Abstract:
A substantially homogeneous calcium/aluminium alloy having a calcium/aluminium atomic ratio of from about 60/40 to 80/20 and with useful and unexpected properties of brittleness, passivity to atmospheric moisture and low volatility is prepared by a process which comprises adding aluminium under an inert atmosphere to molten calcium at a temperature of from about 550 to 1100°C and at a rate to prevent substantial solids formation in the melt during the addition. The molten alloy is converted to particulate solid either by melt atomization or by casting, crushing and grinding. Lead/calcium/aluminum and tin/calcium/aluminum alloys are prepared by adding the calcium/aluminum alloy to the molten lead or tin, while cal- cium/aluminumllithium alloy is prepared by adding lithium to the molten calcium/aluminum alloy.

Inventors:
DEBITSUDO MAAKU DOUDETSUKU
MAAKU ANDORIYUU RAMUBAATO
Application Number:
JP3812283A
Publication Date:
October 04, 1983
Filing Date:
March 08, 1983
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
PFIZER
International Classes:
C22C1/02; C22C1/03; C22C21/00; (IPC1-7): C22C1/02; C22C21/00
Domestic Patent References:
JP38006357A
Attorney, Agent or Firm:
Hideto Asamura