ALUMINUM ALLOY AND ALUMINUM ALLOY WIRE
Document Type and Number:
Japanese Patent JP2014125665
Kind Code:
A
Abstract:
PROBLEM TO BE SOLVED: To provide an aluminum alloy having high strength and excellent in brightness after an anodic oxidation treatment, and to provide an aluminum alloy wire.SOLUTION: There is provided an aluminum alloy containing Mg of 4.5 mass% to 12.0 mass% and the balance Al with inevitable impurities and has the content of hydrogen of 10 ml/100 g or less. A crystallized and precipitated product having a diameter of 10 μm or more on a cross section of the aluminum alloy is 3/mmor less. The aluminum alloy is excellent in strength because it contains a lot of Mg, and can prevent degradation of appearance due to a blowhole because the content of hydrogen is in a specific range. Also the aluminum alloy is excellent in brightness after an anodic oxidation treatment because there is little coarse crystallized and precipitated products.

Inventors:
TANJI AKIRA
NISHIKAWA TAICHIRO
NAKAI YOSHIHIRO
AZUMA KENJI
TAKIGAWA NOBUYASU
UESUGI NORITERU
Application Number:
JP2012284696A
Publication Date:
July 07, 2014
Filing Date:
December 27, 2012
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
SUMITOMO ELECTRIC INDUSTRIES
UNIV OSAKA PREFECTURE
International Classes:
C22C21/00; C22C21/06; C22F1/00; C22F1/047
Domestic Patent References:
JP2007100205A2007-04-19
JP2012229485A2012-11-22
JP2008255371A2008-10-23
JPS63216953A1988-09-09
JP2005344173A2005-12-15
JPH04218635A1992-08-10
JP2012082469A2012-04-26
JP2007100205A2007-04-19
JP2012229485A2012-11-22
JP2008255371A2008-10-23
Other References:
JPN6016022602; 40周年記念事業実行委員会 記念出版部会: アルミニウムの組織と性質 , 19911130, 第376-379頁, 軽金属学会
Attorney, Agent or Firm:
Hiroshi Yamano