PURPOSE: To obtain a thermoplastic compound having high impact strength and good heat stability by making respectively prescribed amounts of an aromatic poly(ether sulfone) of a high deflection temperature under load, a poly-α- methtylstyrene, a specified graft copolymer be contained.
CONSTITUTION: An aromatic poly(ether sulfone) of a high deflection temperature under load [example: reaction product between 2,2-bis(4-hydroxyphenyl)-propane and bis(4-chlorophenyl)-sulfone] (5-99 pts.wt.), 5-95 pts.wt. of a poly-α- methylstyrene (example: α-methylstyrene-acrylonitrile-acrylamide terpolymer), and 1-95 pts.wt. of a graft copolymer in which a resin forming monomer (example: styrene, acrylonitrile) is grafted on rubber (example: polybutadiene rubber) are incorporated.