Abstract:
Ni base superalloy components containing relatively large amounts of Al and Ti are known to be difficult to build up by a weld build up process without cracking. As the Al and Ti content of the superalloy is increased to improve the strength, the susceptibility to cracking is increased. It is shown herein that reducing the Gamma' phase in the additive built up material improves robustness against cracking. A stepwise, controlled heating and cooling process is described to be used in cooperation with an additive build up process to reduce the Gamma' present and thereby reduce cracking.

Inventors:
Kazim Ozbaisal
Application Number:
JP2015511797A
Publication Date:
October 12, 2016
Filing Date:
May 13, 2013
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
Siemens Energy Incorporated
International Classes:
B23K26/34; B23K15/00; B23K26/21; B23K26/342; F01D5/28; F01D25/00; F02C7/00
Domestic Patent References:
JP5192785A
JP2002524268A
JP2011083822A
JP2011214541A
JP2001269784A
JP9506039A
Foreign References:
US4804815
US6124568
US20020148817
Attorney, Agent or Firm:
Yasuhiko Murayama
Takashi Watanabe
Shinya Mitsuhiro