Abstract:
A method for producing hardened parts of steel from an air-hardening steel comprising the steps of heating the steel is heated to a temperature above 1,100° C., hot-working the steel parts until they reach the A1 emperature, cooling the steel parts in air to about 280° C. under simultaneous thermo-mechanical sizing treatment, then cooling the steel parts in air to room temperature, stress relief treating the steel parts at 150-250° C., and hard-machining the steel parts.
More Like This:
WO/2016/013424 | COOLING DEVICE AND MULTI-CHAMBER HEAT TREATMENT DEVICE |
WO/2012/043837 | PRESS-MOLDED ARTICLE AND METHOD FOR PRODUCING SAME |
Inventors:
Frank hengerel
Application Number:
JP13027399A
Publication Date:
October 13, 2010
Filing Date:
May 11, 1999
Export Citation:
Assignee:
SKF GESELLSCHAFT MIT BESCHANKTER HAFTUNG
International Classes:
C21D1/18; C21D8/00; C21D1/30; C22C38/00; C22C38/46; C21D9/32; C21D9/40
Domestic Patent References:
JP55049127B1 | ||||
JP9242763A | ||||
JP4280918A | ||||
JP10137888A | ||||
JP3013526A | ||||
JP11309630A |
Foreign References:
US4973368 |
Other References:
大和久 重雄,金属熱処理用語辞典,日本,日刊工業新聞社,1985年10月30日,第84頁
Attorney, Agent or Firm:
Toru Fujioka