To provide a method for coating the surface of a concrete structure, which has excellent workability and by which the hardening property of a surface coating material is not changed seasonally and the swell of the surface coating material and the occurrence of a pinhole are restrained and a cracking phenomenon is not propagated in the hardened surface coating material and to provide a surface-coated structure of the concrete structure.
This method for coating the surface of the concrete structure 1 comprises the steps of forming a surface preparing layer 2 on the surface of the concrete structure 1 and forming a surface protecting layer 3 on the surface of the surface preparing layer 2. The surface preparing layer 2 is formed from a one-component humidity-curable polyurethane resin or two-component-curable polyurethane resin which has 10-300,000 mPas viscosity and 1.0-20.0 thixotropy index. The one-component humidity-curable polyurethane resin or two-component-curable polyurethane resin is applied to/rubbed into the surface of the concrete structure 1. The concrete structure 1 is bonded to the surface preparing layer 2 through a primer.
AOKI JUNICHI
JPS52109519A | 1977-09-13 | |||
JP2003221572A | 2003-08-08 | |||
JP2001342339A | 2001-12-14 | |||
JPH08199061A | 1996-08-06 | |||
JP2001303897A | 2001-10-31 | |||
JPH04219173A | 1992-08-10 |
Tadashi Takahashi
Takashi Watanabe
Masakazu Aoyama
Suzuki Mitsuyoshi
Kazuya Nishi
Yasuhiko Murayama