To provide a thermoplastic resin composition excellent in weatherability, impact resistance and appearance.
The thermoplastic resin composition comprises (I) 50-90 mass% of the continuous phase described below and (II) 10-50 mass% of the disperse phase described below. In this composition, the weight-average molecular weight of the continuous phase is 60,000-200,000 and the volume-average particle size of the disperse phase is 0.3-1.5μm and the graft percentage is ≥20%; wherein, the continuous phase(I) consists of a styrene-(meth)acrylic ester-based copolymer made from a styrene-based monomer, a (meth)acrylic ester-based monomer and optionally a vinyl monomer copolymerizable therewith, and the disperse phase(II) consists of a polymer obtained by grafting a styrene-(meth)acrylic ester-based copolymer made from a styrene-based monomer, a (meth)acrylic ester-based monomer and optionally a vinyl monomer copolymerizable therewith to a polyolefin-based rubbery elastomer ≤-30°C in glass transition temperature.
SHIMIZU KOICHI
DAIKO HIROKI
JPH11263890A | 1999-09-28 | |||
JPH09132619A | 1997-05-20 | |||
JPS62158749A | 1987-07-14 | |||
JPS60231754A | 1985-11-18 | |||
JP2001151974A | 2001-06-05 | |||
JPS62177054A | 1987-08-03 | |||
JPH0423845A | 1992-01-28 | |||
JPH0455455A | 1992-02-24 |