To provide a water shut-off material capable of sufficiently exhibiting water shutting-off performance in a short time.
The water shut-off material contains a solid component containing bentonite and a liquid having a hydrophobic property. When water intrudes into a clearance formed between a plurality of bentonite particles 1 and filled with the hydrophobic liquid, the hydrophobic liquid in the clearance 2 is easily pushed out by water without being mixed therewith, and the hydrophobic liquid in the clearance 2 is replaced by water. Thereby, the bentonite particle 1 is contacted with water in a short time from intrusion of water. Accordingly, the water shut-off material can exhibit the water shutting-off performance in a short time as compared with the conventional water shut-off material in which the bentonite particle 1 is started to be swelled after the hydrophilic liquid near the bentonite particle 1 is sufficiently diluted.
TOIDA KATSU
YOKOZEKI KOSUKE
WATANABE KENZO
JPH06248895A | 1994-09-06 | |||
JP2003213259A | 2003-07-30 | |||
JP2007232388A | 2007-09-13 | |||
JP2008045314A | 2008-02-28 | |||
JPH1076238A | 1998-03-24 | |||
JPH0297771A | 1990-04-10 | |||
JP2003213260A | 2003-07-30 | |||
JPH08169712A | 1996-07-02 | |||
JP2002088344A | 2002-03-27 | |||
JPH09248877A | 1997-09-22 | |||
JPH10338812A | 1998-12-22 | |||
JPH0458840B2 | 1992-09-18 | |||
JPH09100462A | 1997-04-15 | |||
JPH08231956A | 1996-09-10 | |||
JPH0297771A | 1990-04-10 | |||
JP2003213260A | 2003-07-30 | |||
JPH08169712A | 1996-07-02 | |||
JP2002088344A | 2002-03-27 | |||
JPH09248877A | 1997-09-22 | |||
JPH10338812A | 1998-12-22 | |||
JPH0458840B2 | 1992-09-18 | |||
JPH09100462A | 1997-04-15 | |||
JPH08231956A | 1996-09-10 | |||
JPH06248895A | 1994-09-06 | |||
JP2003213259A | 2003-07-30 | |||
JP2007232388A | 2007-09-13 | |||
JP2008045314A | 2008-02-28 | |||
JPH1076238A | 1998-03-24 |
Yoshiki Kuroki
Next Patent: HEAT RESISTANT POLYLACTIC ACID MOLDED PRODUCT AND METHOD FOR PRODUCING IT