Abstract:
Zr—Ti—Ni(Cu)-based filler alloy composition having low melting point for brazing titanium and titanium alloys is expressed as: ZraTibNic (Formula 1) where a, b and c denote atomic % of Zr, Ti and Ni, respectively; 47≰a≰52; 24≰b≰30; 22≰c≰26; and 0.3

Inventors:
Shin Young
Lee Dong Myung
Song Ju Hyun
Kim Young Fan
Kang Dong Han
Application Number:
JP2010519865A
Publication Date:
January 23, 2013
Filing Date:
August 07, 2008
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
KOREA INSTITUTE OF INDUSTRIAL TECHNOLOGY
International Classes:
B23K35/32; C22C16/00; C22C30/02
Domestic Patent References:
JP9118571A
JP11040583A
JP9314358A
JP4238877A
JP59126739A
Attorney, Agent or Firm:
Ichiro Kudo



 
Previous Patent: JPS5123385

Next Patent: DEODORANT AND ITS MANUFACTURE