Title:
ADDITION-CURABLE SILICONE RUBBER COMPOSITION AND CURED SILICONE RUBBER PRODUCT
Document Type and Number:
WIPO Patent Application WO/2023/276628
Kind Code:
A1
Abstract:
The present invention provides an addition-curable silicone rubber composition which is characterized by containing: 100 parts by mass of (A) an alkenyl group-containing organopolysiloxane that has an alkenyl group bonded to two or more silicone atoms in each molecule; 0.2 to 20 parts by mass of (B) an organohydrogen polysiloxane that has two or more hydrogen atoms, each of which is bonded to a silicon atom, in each molecule; a catalytic amount of (C) a platinum-based catalyst; 0.01 to 5.0 parts by mass of (D) a thermally dissociative blocked (poly)isocyanate; and 0.01 to 10.0 parts by mass of (E) a heat resistance imparting agent. Consequently, the present invention provides: an addition-curable silicone rubber composition which enables the achievement of a cured product which has a low compression set even under high temperature conditions of 200°C or more; and a cured silicone rubber product.
Inventors:
HARA TATSUEI (JP)
KATO NOBU (JP)
UBUKATA SHIGERU (JP)
KATO NOBU (JP)
UBUKATA SHIGERU (JP)
Application Number:
PCT/JP2022/023581
Publication Date:
January 05, 2023
Filing Date:
June 13, 2022
Export Citation:
Assignee:
SHINETSU CHEMICAL CO (JP)
International Classes:
C08L83/07; C08K3/04; C08K3/22; C08K3/36; C08K5/205; C08K5/29; C08L83/05
Foreign References:
JP2019006952A | 2019-01-17 | |||
JP2019006956A | 2019-01-17 | |||
JP2019147909A | 2019-09-05 | |||
JP2020070357A | 2020-05-07 | |||
JP2010009903A | 2010-01-14 | |||
JPH03100059A | 1991-04-25 | |||
JP2009158481A | 2009-07-16 | |||
JP2016518461A | 2016-06-23 | |||
JP2014031408A | 2014-02-20 | |||
JP2017165931A | 2017-09-21 | |||
JP2019006956A | 2019-01-17 | |||
JP2020070357A | 2020-05-07 |
Attorney, Agent or Firm:
YOSHIMIYA Mikio et al. (JP)
Download PDF: