Abstract:
An application of heat-resistant explosion-proof glassware having a low difference value of a high-temperature region thermal expansion coefficient, a low crystallization speed, and a high softening point, wherein the glass contains 0.01%-39% of aluminum oxide and 7%-20% of magnesium oxide according to percentage by weight; the content of silicon oxide is 2.51-4.8 times greater than that of calcium oxide; the content of calcium oxide is 0.7-2.3 times greater than that of magnesium oxide. The glassware has a softening point of 750℃-940℃ and a breaking strength of 70-240 MPa.
Inventors:
YANG DENING (CN)
Application Number:
PCT/CN2015/000794
Publication Date:
May 26, 2017
Filing Date:
November 16, 2015
Export Citation:
Assignee:
YANG DENING (CN)
International Classes:
C03C3/087
Foreign References:
CN102234181A | 2011-11-09 | |||
CN102557459A | 2012-07-11 |
Download PDF:
Previous Patent: VEHICLE BUMPER COMPRISING MULTIPLE DAMPING AND ENERGY ABSORBING SHIELDS THEREIN
Next Patent: METHOD FOR MANUFACTURING GLASSES FRAME
Next Patent: METHOD FOR MANUFACTURING GLASSES FRAME