Title:
BIAXIALLY ORIENTED POLYETHYLENE TEREPHTHALATE FILM AND METHOD FOR PRODUCING SAME
Document Type and Number:
WIPO Patent Application WO/2014/030474
Kind Code:
A1
Abstract:
This film provides a polyethylene terephthalate film whereby dimensional variation in various steps can be reduced, particularly when the film is used as a substrate film for a flexible device, and that is suitable as a substrate film having minimal curl and excellent appropriateness for processing. This biaxially oriented polyethylene terephthalate film has a degree of crystallinity (Xc) of 0.35 to 0.50, the intrinsic viscosity (IV) of the resin constituting the film is 0.66-1.0 dl/g, the coefficient of thermal expansion at a temperature of 50-170°C in each of the longitudinal direction and width direction of the film is 0.29 ppm/°C, and the thermal shrinkage at 180°C in each of the longitudinal direction and width direction of the film is 0.5%-1.0%.
More Like This:
JPH0847972 | BIAXIALLY ORIENTED POLYAMIDE FILM AND PRODUCTION THEREOF |
JPS5627326 | MANUFACTURE OF FILM FOR TAPE |
JPS58194016 | 【考案の名称】2軸延伸機チヤツク |
Inventors:
TAKAHASHI KENTA (JP)
MACHIDA TETSUYA (JP)
HIGASHIOJI TAKUJI (JP)
MACHIDA TETSUYA (JP)
HIGASHIOJI TAKUJI (JP)
Application Number:
PCT/JP2013/069620
Publication Date:
February 27, 2014
Filing Date:
July 19, 2013
Export Citation:
Assignee:
TORAY INDUSTRIES (JP)
International Classes:
B29C55/12; C08J5/18; B29K67/00; B29L7/00; B29L31/34
Domestic Patent References:
WO2012114988A1 | 2012-08-30 |
Foreign References:
JPH10138333A | 1998-05-26 | |||
JP2010270237A | 2010-12-02 | |||
JPH09323394A | 1997-12-16 | |||
JP2000309052A | 2000-11-07 | |||
JP2008030475A | 2008-02-14 | |||
JP2012136016A | 2012-07-19 | |||
JP2011178866A | 2011-09-15 |
Download PDF:
Previous Patent: INK COMPOSITION, IMAGE FORMING METHOD, PRINTED MATTER, AND GRAFT COPOLYMER
Next Patent: SPECTROPHOTOMETER
Next Patent: SPECTROPHOTOMETER