Abstract:
This ferrite austenite 2-phase stainless steel plate comprises, by mass%, C: 0.001-0.10%, Si: 0.01-1.0%, Mn: 2-10%, P < 0.05%, Ni: 0.1-3.0%, Cr: 15.0-30.0%, and N: 0.05-0.30%, with the remainder being Fe and inevitable impurities. The austenite phase percentage is 40-90% by surface area percentage, the maximum strength of the crystal orientation of the ferrite phase is 10 or less, and the hardness ratio of the austenite phase to the ferrite phase is 1.1 or greater.
More Like This:
Inventors:
HAMADA JUNICHI (JP)
ISHIMARU EIICHIRO (JP)
ISHIMARU EIICHIRO (JP)
Application Number:
PCT/JP2013/055945
Publication Date:
September 12, 2013
Filing Date:
March 05, 2013
Export Citation:
Assignee:
NIPPON STEEL & SUMIKIN SST (JP)
International Classes:
C22C38/00; C21D9/46; C22C38/58
Foreign References:
JP2009035782A | 2009-02-19 | |||
JP2009197326A | 2009-09-03 | |||
JP2010121162A | 2010-06-03 | |||
JP2011184792A | 2011-09-22 | |||
JP2011208244A | 2011-10-20 |
Attorney, Agent or Firm:
SHIGA Masatake et al. (JP)
Masatake Shiga (JP)
Masatake Shiga (JP)
Download PDF:
Claims:
Previous Patent: ANTIBODY PURIFICATION METHOD, AND CARRIER FOR USE IN PURIFICATION OF ANTIBODY
Next Patent: SUSPENSION DEVICE
Next Patent: SUSPENSION DEVICE