Abstract:
This hot-rolled ferritic stainless steel sheet has a composition containing, in mass%, up to 0.0150 % of C, 0.01 to 2.00 % of Si, 0.01 to 2.00% of Mn, less than 0.040% of P, up to 0.010% of S, 10.0 to 30.0% of Cr, 0.001 to 0.100% of Al and up to 0.0200% of N with the balance being Fe and unavoidable impurities, and satisfies the relationship: La/L ≥ 0.20 [wherein L is the length of all grain boundaries with misorientation angles of 1 to less than 180° as observed in a section in the range of 1/4 to 3/4 of the sheet thickness and La is the length of subgrain boundaries with misorientation angles of 1 to less than 15° as observed therein].

Inventors:
KIMURA KEN (JP)
HAMADA JUNICHI (JP)
TAKAHASHI JUN (JP)
KOYAMA YUUJI (JP)
GOTOH SHIGEYUKI (JP)
Application Number:
PCT/JP2012/081693
Publication Date:
June 13, 2013
Filing Date:
December 06, 2012
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
NIPPON STEEL & SUMIKIN SST (JP)
International Classes:
C22C38/00; B21B3/02; C21D9/46; C22C38/38; C22C38/58
Foreign References:
JP2004270026A2004-09-30
JP2010100877A2010-05-06
JPH10237602A1998-09-08
JPH08199237A1996-08-06
JP2012140687A2012-07-26
Attorney, Agent or Firm:
SHIGA Masatake et al. (JP)
Masatake Shiga (JP)
Download PDF:
Claims: