Abstract:
A method for correcting the inner diameter of a pipe end of a seamless pipe formed from high-CR stainless steel containing 8 to 35 mass% of CR and 0.1 to 10 mass% of Ni comprises: a pipe end correction step with which the pipe end part of a seamless pipe is enlarged by inserting a plug for inner diameter correction into the pipe end part after a step for pipe production by hot working and a heat treatment step, when oxide scale build-up is generated on the inside surface at the pipe end part of a seamless pipe; and a step for forming a lubricant film with which, prior to this pipe end correction step, a lubricant is applied to the inside surface at the pipe end part of a seamless pipe and/or the plug surface to form a lubricant film. As a result, the formation of seizure marks on the inside of the pipe end part can be prevented when a high-CR stainless steel seamless pipe is produced.

Inventors:
MOCHIZUKI TOSHIO (JP)
Application Number:
PCT/JP2012/000948
Publication Date:
August 23, 2012
Filing Date:
February 14, 2012
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
SUMITOMO METAL IND (JP)
MOCHIZUKI TOSHIO (JP)
International Classes:
B21B23/00; B21D41/02; B21B25/04; B21D3/14; C10M105/24; C22C38/00; C22C38/46; C10N10/02; C10N30/00; C10N40/24
Domestic Patent References:
WO2007132851A12007-11-22
WO2007114176A12007-10-11
Foreign References:
JP2010142810A2010-07-01
JPS635807A1988-01-11
JPH044906A1992-01-09
JP2006000916A2006-01-05
JP2006181611A2006-07-13
JP2010142810A2010-07-01
Other References:
See also references of EP 2676747A4
Attorney, Agent or Firm:
MORI, Michio et al. (JP)
Woods Michio (JP)
Download PDF:
Claims: