Title:
コージェライト質セラミックハニカム構造触媒用担体及びその製造方法
Document Type and Number:
Japanese Patent JP3587365
Kind Code:
B2
Abstract:
PROBLEM TO BE SOLVED: To obtain a lightweight honeycomb structure which is light in comparison with other honeycomb structures even when the thickness is the same by increasing porosity in the cell wall and to obtain a catalyst carrier having a ceramic honeycomb structure, which can be rapidly heated and has sufficient mechanical strengths. SOLUTION: The catalyst carrier having the cordierite-based ceramic honeycomb structure is characterized by that the volume of pores having diameters of 0.5 to 2 μm is >=30% of the total pore volume, the volume of pores having diameters of 5 to 10 μm is <=20% of the total pore volume, the volume of pores having diameters of <=10 μm is <=30% of the total pore volume, the porosity is >=35%, the A-axis compressive strength is >=18 MPa and the mass per carrier volume containing cell spaces is <=400 g/l.

Inventors:
Yasuhiko Otsubo
Junichi Suwabe
Application Number:
JP2000159824A
Publication Date:
November 10, 2004
Filing Date:
May 30, 2000
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
Hitachi Metals Co., Ltd.
International Classes:
B01J32/00; B01J35/04; C04B35/195; (IPC1-7): B01J35/04; B01J32/00; C04B35/195
Domestic Patent References:
JP2000239059A
JP5085813A
JP63197550A
Foreign References:
EP0894777A1