Abstract:
1. Process for forming at least one sparingly soluble metal salt in a reaction vessel by mixing at least one solution A, which contains at least one cation of the metal salt, with at least one solution B, which contains at least one anion of the metal salt, by running at least one of these solutions into a reaction vessel, characterized in that this solution is run in for at least part of the process in such a way that the concentration of the inflowing solution continuously changes.
Inventors:
HAINTSU TAITOSHAITO
UIRUHERUMU ZAAREKU
HAARARUTO FUON RINTEREN
UIRUHERUMU ZAAREKU
HAARARUTO FUON RINTEREN
Application Number:
JP6799480A
Publication Date:
December 09, 1987
Filing Date:
May 23, 1980
Export Citation:
Assignee:
AGFA GEVAERT AG
International Classes:
B01D9/02; B01J14/00; C01G1/00; C01G5/02; G03C1/005; G03C1/015
Previous Patent: A detecting method of biological activity
Next Patent: GENERATING METHOD FOR BIT MAP FONT
Next Patent: GENERATING METHOD FOR BIT MAP FONT