To provide a polyester fiber having improved abrasion resistance which is a problem in prior arts, and most suitable for apparel use, especially for woven or knitted fabric to use a fine-denier fiber: and to provide a method for producing the polyester fiber.
The polyester fiber is produced by melt-spinning of a polyester containing ethylene terephthalate as a main repeating unit and satisfies the following requirements (1) to (5). (1) The fineness is ≥8 dtex and ≤100 dtex; (2) the single fiber fineness is ≥1 dtex and ≤4 dtex; (3) the breaking strength is ≥4 cN/dtex; (4) the breaking elongation is ≥20% and ≤50%; and (5) the minimum differential Young's modulus is ≤20 cN/dtex in an elongation range of ≥2% and ≤5% on a stress-strain curve of the fiber.
YAMASHITA AKIRA
JP2001207329A | 2001-08-03 | |||
JPH03124876A | 1991-05-28 | |||
JPS6221832A | 1987-01-30 | |||
JP2001164423A | 2001-06-19 | |||
JP2008101295A | 2008-05-01 | |||
JPS62104942A | 1987-05-15 | |||
JP2004027415A | 2004-01-29 | |||
JP2005002496A | 2005-01-06 | |||
JP2005194669A | 2005-07-21 | |||
JPH09143816A | 1997-06-03 | |||
JPH08100347A | 1996-04-16 | |||
JPH06280114A | 1994-10-04 | |||
JP2004270061A | 2004-09-30 |
Takashi Ishida
Tetsuji Koga
Kazuhiro Nakamura
Hiroyuki Onoda
Toko Saito