PURPOSE: To obtain excellent demisting property and scratch resistance of the subject plastic by a method in which the metallic oxide-layer treated with specified treatment liquid is provided on one surface of plastic base, and an adhesive layer is provided on the other surface thereof.
CONSTITUTION: A metallic oxide layer is formed on one surface of a plastic base. As the material constituting the metallic oxide, e.g. SiO2, SiO, Al2O3, MgO, ZrO2, CaO, TiO2, SnO2, In2O3, WO3, MoO3, BaO, ZnO, NiO, HfO2 or Ta2O3, etc., is used. The metallic oxide layer is treated with the treatment liquid containing the aliphatic hydrocarbon having at least one hydroxy group and the functional group except hydroxy group and/or the aliphatic hydrocarbon having at least three hydroxy group and no functional group except hydroxy group. The adhesive layer provided on the other surface of the plastic base is formed by coating its surface with the adhesive such as acryl group, urethane group, silicon group or rubber group, etc. The demisting plastic thus made may be used in sticking said adhesive surface-layer to the surface of glass or plastic.
YUASA MOTOKAZU
UEHARA TAKESHI
TSUTAO TOMOSHIGE
FUKUMOTO YOSHIYUKI