Abstract:

PURPOSE: To produce a material having a good electromagnetic shielding effect, by mixing a thermoplastic resin having a specified particle size with an electrically conductive fibrous filler in a rotating container type mixer and extruding the mixture.

CONSTITUTION: Thermoplastic resin particles having a particle size of 2mm or below, such as polyolefin or polystyrene particles, and 5W80wt% (based on the total quantity of the compsn.) electrically conductive fibrous filler having a fiber length of 0.5W10mm and a fiber diameter of 10W200μ, such as metallic fiber, carbon fiber or metal-coated glass fiber, are mixed together in a rotating container type mixer such as a tumbler. The resulting mixture is extruded through an extruder (pref. one having a full-flighted screw) to form pellets, thus obtaining the titled electromagnetic shielding material.


Inventors:
NISHIMURA KATSUMI
MIYASHITA SUSUMU
OOTA NAOKI
SUGIURA MAKOTO
Application Number:
JP21826082A
Publication Date:
June 25, 1984
Filing Date:
December 15, 1982
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
TOYO INK MFG CO
International Classes:
C08K7/00; C08K7/04; C08L1/00; C08L7/00; C08L21/00; C08L23/00; C08L27/00; C08L33/00; C08L33/02; C08L51/00; C08L51/02; C08L67/00; C08L77/00; C08L101/00; H05K9/00; (IPC1-7): C08K7/04; H05K9/00



 
Previous Patent: JPS59109536

Next Patent: RADIAL-PLY TIRE