To obtain an improved bead shape in which no humping, undercut and underfill are generated when welding is performed for a steel material with a low molten metal viscosity.
In a two-welding wire feeding arc welding method, a first (preceding) welding wire 11 and a second (succeeding) welding wire 12 insulated from each other are supplied from the nozzle 6 at the tip end of a welding torch to weld a steel material with a low molten metal viscosity. In this method, a welding current Iw is energized in the preceding welding wire to generate an arc 3 to form a molten pool 21 while no welding current is energized in the succeeding welding wire. The succeeding welding wire is inserted in a position rising after the molten pool 21 is dug down by the pressure of the arc 3, in the two welding wire feeding arc welding method.
OONAWA TOSHIO
MITA TSUNEO
JPH0663754A | 1994-03-08 | |||
JPS5245555A | 1977-04-11 |