Abstract:
A method of mitigating against thermal contraction induced cracking during casting of a super Ni alloy, the method comprising: pouring liquid alloy into a mould such that liquid alloy is present in a feeder of said mould; and inducing an electrical current in alloy in said feeder to reduce a rate of cooling of alloy in said feeder.

Inventors:
Goodwin, Richard, Stanley
Roberts, Stefan
Application Number:
JP2011505586A
Publication Date:
September 04, 2013
Filing Date:
April 24, 2009
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
GOODWIN PLC
International Classes:
B22D27/06; B22C9/08; B22D7/10; B22D21/00
Domestic Patent References:
JP55001984A
JP9314310A
JP61286054A
JP55064958A
Attorney, Agent or Firm:
Longhua International Patent Service Corporation



 
Previous Patent: JPS5282813

Next Patent: テープカセット