Abstract:
These fibers with thermal elongation properties comprise a first resin component, and a second resin component having a melting point or a softening point that is lower than the melting point of the first resin component, and at least part of the fiber surface of the second resin component is continuously present in the length direction, and the length extends as a result of applying heat. The rate of change ({(B - A)/A} × 100) of the thermal elongation B at the melting point of the second resin component plus 10°C with respect to the thermal elongation A at the melting point of the second resin component minus 6°C is at least 130%. The first resin component preferably comprises polylactic acid, while the second resin component preferably comprises a polyolefin. The ratio (crimp rate (%)/number of crimps (count)) between the crimp rate (%) measured in accordance with JIS L1015 and the number of crimps (count) measured in accordance with JIS L1015 is preferably between 0.45 and 0.75.

Inventors:
NAGASHIMA KEISUKE (JP)
TANEICHI SHOICHI (JP)
Application Number:
PCT/JP2012/077707
Publication Date:
May 16, 2013
Filing Date:
October 26, 2012
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
KAO CORP (JP)
NAGASHIMA KEISUKE (JP)
TANEICHI SHOICHI (JP)
International Classes:
D01F8/14; D01F8/06; D04H1/541; D04H1/76
Foreign References:
JP2008101285A2008-05-01
JP2007182662A2007-07-19
JP2007204902A2007-08-16
JP2009114613A2009-05-28
Attorney, Agent or Firm:
HATORI, Osamu et al. (JP)
Osamu Hatori (JP)
Download PDF:
Claims:



 
Previous Patent: LITHIUM ION SECONDARY BATTERY

Next Patent: MACHINE TOOL