Abstract:
The present invention disclosed a method of preparing chromic oxide and ferrous
oxalate from carbon ferrochrome. The carbon ferrochrome which is cheap and gained
easily is used as starting material. The carbon ferrochrome is dissolved in sulfuric
acid, then oxalic acid is added to the solution to separate chrome and iron, and
then ferrous oxalate powder with total impurities content less than 1% and chromic
oxide with iron content less than 0.5% are obtained. The technical conditions
are controlled as following: sulfuric acid of 20%-60% is used to dissolve carbon
ferrochrome, the dissolving temperature is 80-150 °C, the amount of oxalic
acidadded is 105% - 120% of the theoretical amount to precipitate iron into ferrous
oxalate, precipitation time of iron is 20 min - 1h, and precipitation pH of iron
is 2.0 - 4.0.
Inventors:
HU GUOHUA (CN)
Application Number:
PCT/CN2008/000084
Publication Date:
August 07, 2008
Filing Date:
January 11, 2008
Export Citation:
Assignee:
HUNAN JOYFLY TECHNOLOGY DEV CO (CN)
HU GUOHUA (CN)
HU GUOHUA (CN)
International Classes:
C01G37/033; C01G49/00; C07C51/41; C07C55/07; C22B34/32
Foreign References:
CN101041466A | 2007-09-26 | |||
JPS5238472A | 1977-03-25 | |||
US4608084A | 1986-08-26 |
Other References:
See also references of EP 2116515A4
Attorney, Agent or Firm:
CHANGSHA ZONEKEY PATENT LAW FIRM (Changsha, Hunan 1, CN)
Download PDF:
Previous Patent: STEREO VIDEO MULTIMEDIA MOBILE TELEPHONE
Next Patent: METHOD OF PRINTING TEXTURE ON WOODY WINDOW BLIND SLATS
Next Patent: METHOD OF PRINTING TEXTURE ON WOODY WINDOW BLIND SLATS