Title:
POLYARYLENE SULFIDE RESIN COMPOSITION AND MOLDED ARTICLE COMPRISING SAME
Document Type and Number:
WIPO Patent Application WO/2015/098748
Kind Code:
A1
Abstract:
A polyarylene sulfide resin composition obtained by combining 0.001-10 mol% of (B) an organic carboxylic acid alkaline earth metal salt with respect to the formula –(Ar-S)-, which is a repeating unit of polyarylene sulfide, with respect to (A) polyarylene sulfide, wherein the weight-average molecular weight of the (A) polyarylene sulfide is 10,000 or higher and the weight loss on heating of the polyarylene sulfide resin composition satisfies the following formula. ΔWr = (W1 - W2)/W1 × 100 ≦ 0.18(%) (where ΔWr is the weight loss rate (%), which is a value determined from the sample weight upon reaching 330°C (W2) with respect to the sample weight upon reaching 100°C (W1) when thermogravimetric analysis is conducted at a heating rate of 20°C/min from 50°C to any temperature of 330°C or above in a normal-pressure non-oxidizing atmosphere). Provided is a polyarylene sulfide resin composition having a lowered crystallization temperature, suppressed solidification rate, and low gas generation under high temperature, using polyarylene sulfide obtained by a simple, economical method.
Inventors:
ICHINOSE KEIKO (JP)
TAKAO HIDENOBU (JP)
YAMAMOTO DAISUKE (JP)
YAMAUCHI KOJI (JP)
TAKAO HIDENOBU (JP)
YAMAMOTO DAISUKE (JP)
YAMAUCHI KOJI (JP)
Application Number:
PCT/JP2014/083698
Publication Date:
July 02, 2015
Filing Date:
December 19, 2014
Export Citation:
Assignee:
TORAY INDUSTRIES (JP)
International Classes:
C08L81/02; C08G75/06; C08J3/20; C08K5/098
Domestic Patent References:
WO2007034800A1 | 2007-03-29 | |||
WO2007034800A1 | 2007-03-29 | |||
WO2008105438A1 | 2008-09-04 |
Foreign References:
JPH10195197A | 1998-07-28 | |||
JPS63178164A | 1988-07-22 | |||
JP2005225931A | 2005-08-25 | |||
JPS63178164A | 1988-07-22 | |||
JP2011173953A | 2011-09-08 | |||
JP2012176607A | 2012-09-13 |
Other References:
See also references of EP 3088470A4
Download PDF: