STAINLESS STEEL WIRE, SPRING, AND METHOD FOR PRODUCING SPRING
Document Type and Number:
WIPO Patent Application WO/2005/040443
Kind Code:
A1
Abstract:
A stainless steel wire, which has a chemical composition, in mass %, that C: 0.01 to 0.25, N: 0.01 to 0.25, Mn: 0.4 to 4.0, Cr: 16 to 25, Ni: 8.0 to 14.0 and the balance: Fe and inevitable impurities, with the proviso that C and N satisfy the formula: 0.15 mass % ≤ C + N ≤ 0.35 mass %, and comprises 15 volume % or less of a martensite phase induced by drawing the balanced percentage of an austenite phase and also comprises a texture wherein diffraction intensities of the austenite phase by the X-ray diffraction method in the longitudinal direction of the steel wire satisfy both the formulae: I (200)/I(111) ≥ 2.0 and I (220)/I(111) ≥ 3.0. The stainless steel wire is excellent in both corrosion resistance and fatigue strength and also can be produced with good productivity.
Inventors:
IZUMIDA HIROMU (JP)
KAWABE NOZOMU (JP)
FUJINO YOSHIRO (JP)
MURAI TERUYUKI (JP)
TAKAMURA SHINEI (JP)
KAWABE NOZOMU (JP)
FUJINO YOSHIRO (JP)
MURAI TERUYUKI (JP)
TAKAMURA SHINEI (JP)
Application Number:
PCT/JP2004/016041
Publication Date:
May 06, 2005
Filing Date:
October 28, 2004
Export Citation:
Assignee:
SUMITOMO SEI STEEL WIRE CORP (JP)
IZUMIDA HIROMU (JP)
KAWABE NOZOMU (JP)
FUJINO YOSHIRO (JP)
MURAI TERUYUKI (JP)
TAKAMURA SHINEI (JP)
IZUMIDA HIROMU (JP)
KAWABE NOZOMU (JP)
FUJINO YOSHIRO (JP)
MURAI TERUYUKI (JP)
TAKAMURA SHINEI (JP)
International Classes:
B21C1/00; C21D1/26; B21F35/00; C21D9/02; C22C38/00; C22C38/58; C21D8/06; (IPC1-7): C22C38/00; C22C38/58; C21D9/02
Foreign References:
JP2003226940A | 2003-08-15 | |||
JPH09202942A | 1997-08-05 | |||
JP2003034848A | 2003-02-07 | |||
JP2003231919A | 2003-08-19 |
Other References:
See also references of EP 1690955A4
Attorney, Agent or Firm:
Yamano, Hiroshi (10F ASTRO Shin Osaka 2 Bldg., 1-3,
Nishinakajima 6-chome, Yodogawa-k, Osaka-shi Osaka 11, JP)
Download PDF: