Title:
SYNTHETIC GRAPHITE MATERIAL, SYNTHETIC GRAPHITE MATERIAL PRODUCTION METHOD, NEGATIVE ELECTRODE FOR LITHIUM ION SECONDARY BATTERY, AND LITHIUM ION SECONDARY BATTERY
Document Type and Number:
WIPO Patent Application WO/2020/149250
Kind Code:
A1
Abstract:
A synthetic graphite material wherein the crystal grain size L(112) in the c-axis direction as calculated from a (112) diffraction line obtained by wide-angle X-ray diffraction is 4-30nm, the surface area based on volume as calculated by a laser diffraction-type particle size distribution measurement device is 0.22-1.70m2/cm3, the oil absorption is 67-147mL/100g, the spectra derived from carbon that appear in an electron spin resonance method measured by using the X band is within the range 3200-3410gauss, and ΔHpp, which is the spectral line width calculated from the first derivative spectra for said spectra at the temperature of 4.8K, is 41-69gauss.
More Like This:
Inventors:
SUZUKI TAKASHI (JP)
MAEDA TAKASHI (JP)
KARAKANE MITSUO (JP)
SHIRAI TAKAHIRO (JP)
KAWACHI HIROSHI (JP)
KIUCHI NORIYUKI (JP)
MAEDA TAKASHI (JP)
KARAKANE MITSUO (JP)
SHIRAI TAKAHIRO (JP)
KAWACHI HIROSHI (JP)
KIUCHI NORIYUKI (JP)
Application Number:
PCT/JP2020/000810
Publication Date:
July 23, 2020
Filing Date:
January 14, 2020
Export Citation:
Assignee:
JXTG NIPPON OIL & ENERGY CORP (JP)
International Classes:
C01B32/205; B01J27/19; C10B57/04; C10G45/08; H01M4/587
Domestic Patent References:
WO2012020816A1 | 2012-02-16 |
Foreign References:
JP2017019915A | 2017-01-26 | |||
JP2012128973A | 2012-07-05 | |||
JP2016164862A | 2016-09-08 | |||
JP2012216545A | 2012-11-08 | |||
JP2019004664A | 2019-01-10 | |||
JPS5415684B2 | 1979-06-16 | |||
JP2013209528A | 2013-10-10 | |||
JP2013209529A | 2013-10-10 |
Other References:
CARBON, no. 47, 1966
See also references of EP 3912959A4
See also references of EP 3912959A4
Attorney, Agent or Firm:
TANAI Sumio et al. (JP)
Download PDF: