Abstract:
An aluminum alloy comprising 0.0001 mass % to 0.03 mass % of copper, 0.0005 mass % to 0.2 mass % of silicon, 0.5 mass % to 4 mass % of Mn, 0.5 mass % to 3 mass % of Fe, the balance being aluminum and inevitable impurities; and an aluminum alloy further comprising at least one member of 0.01 mass % to 0.5 mass % of Cr, 0.01 mass % to 0.5 mass % of Ti and 0.01 mass % to 0.5 mass % of Zr. A method for manufacturing an aluminum alloy foil which comprises heating an aluminum alloy to a temperature from 350°C to 580°C, subjecting the alloy in an ingot form to a hot rolling of a starting temperature of 350°C to 530°C immediately after the above heating or after keeping the alloy ingot at a temperature from 350°C to 580°C for a time up to 15 hr, and then subjecting the resultant sheet to a cold rolling, followed by subjecting to a softening treatment.

Inventors:
RO AKINORI (JP)
ABE MASAAKI (JP)
HASHIZUME YOSHIKI (JP)
Application Number:
PCT/JP2000/004435
Publication Date:
January 18, 2001
Filing Date:
July 03, 2000
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
TOYO ALUMINIUM KK (JP)
RO AKINORI (JP)
ABE MASAAKI (JP)
HASHIZUME YOSHIKI (JP)
International Classes:
C22C21/00; C22F1/04; (IPC1-7): C22C21/00
Foreign References:
JPS61257459A1986-11-14
JPS62250143A1987-10-31
JPH07318084A1995-12-08
JPS62149857A1987-07-03
JPS5197517A1976-08-27
JPS627826A1987-01-14