Abstract:
A method for producing a micron-size spherical silica aerogel having a selectable or controllable average particle size, the method includes producing a surface—modified silica sol by adding a first organosilane compound to a aqueous acid-silica sol, which comprises an inorganic acid and a water glass solution, with a pH less than 3, dispersive mixing a non-polar organic solvent, a second organosilane compound, and the surface-modified silica sol, at a selected stirring rate which is inversely related to an average particle size, without adding any surfactant or dispersant, a micron-size spherical silica hydrogel and further a hydrophobic micron-size spherical silica gel are then produced. Following by drying or stirring the hydrophobic micron-size spherical silica gel to obtain a controllable micron-size silica aerogel in a spherical and powder forms, respectively.

Inventors:
YODYINGYONG SUPAN (TH)
Application Number:
PCT/TH2017/000086
Publication Date:
November 01, 2018
Filing Date:
December 08, 2017
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
YODYINGYONG SUPAN (TH)
International Classes:
C01B33/158; C01B33/143; C01B33/148; C01B33/154
Domestic Patent References:
WO2017171279A12017-10-05
Foreign References:
US20130106008A12013-05-02
US20130189521A12013-07-25
US20160280557A12016-09-29
CN101205067B2010-12-15
Other References:
See also references of EP 3562782A4
Attorney, Agent or Firm:
THAVARANUNT, Napawan et al. (TH)
Download PDF: